Research Article
Performance Evaluation of Waste Crumb Rubber/Silica Fume Composite Modified Pervious Concrete in Seasonal Frozen Regions
Table 5
Flexural failure strain of RSFPC.
| Mix ID | Flexural failure strain (με) | 1 | 2 | 3 | Mean | St. dev. |
| WCR4 + SF12 | 1546 | 1482 | 1511 | 1513 | 26 | WCR6 + SF12 | 2194 | 2098 | 2174 | 2155 | 41 | WCR8 + SF12 | 2401 | 2381 | 2375 | 2386 | 11 |
|
|