The average lattice constant of NiO in the milled powders/(Å).
| | 0 h | 0.5 h | 2 h | 5 h | 10 h |
| Lattice constant | | 4.1723 | 4.1721 | 4.1724 | 4.1730 | 4.1725 | a | 5.0342 | 5.02773 | 5.02656 | 5.03301 | 5.03177 | c | 13.746 | 13.74831 | 13.75972 | 13.7505 | 13.7762 |
|
|