Research Article
Synthesis and Characterization of Mechanical Properties of AA8014 + Si3N4/ ZrO2 Hybrid Composites by Stir Casting Process
Table 2
Wear test process parameters and their levels.
| S. No | Parameter | Level 1 | Level 2 | Level 3 |
| 1. | % of reinforcement | 4 | 6 | 8 | 2. | Stir speed (rpm) | 400 | 500 | 600 | 3. | Stir time (min) | 20 | 25 | 30 | 4. | Molten temperature (oC) | 700 | 800 | 900 |
|
|