Research Article

Synthesis of Luminescent Ink from Europium-Doped Y2O3 Dispersed in Polyvinyl Alcohol Solution

Figure 2

SEM images of samples prepared at different heating temperature peaks: (a) 800 oC and (b) 1000 oC. The lengths of the scale bars are 1 μm.
918351.fig.002a
(a)
918351.fig.002b
(b)