Research Article

Synthesis of Luminescent Ink from Europium-Doped Y2O3 Dispersed in Polyvinyl Alcohol Solution

Figure 3

XRD patterns of samples prepared at heating temperature of 800 oC and doping level of 4% mol/mol.
918351.fig.003