Research Article
Effect of Etching Time on Optical and Thermal Properties of p-Type Porous Silicon Prepared by Electrical Anodisation Method
Figure 3
(a) PL peaks for different anodisation time excited by 405 nm and (b) band gap versus etching time/thickness.