Advances in Optical Technologies / 2012 / Article / Fig 9

Research Article

Infrared Camera Analysis of Laser Hardening

Figure 9

The dependence of surface hardness and hardening depth after HPDD laser hardening on scanning velocity of engraving laser by repetition frequency of 30 kHz.
593893.fig.009

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19. Sign up here as a reviewer to help fast-track new submissions.