Research Letter
Electrochemical Behavior of Titanium and Its Alloys as Dental Implants in Normal Saline
Table 2
Corrosion
parameters for the forward and reverse scans for the alloys at after seven days.
| Material | Forward scan | Reverse scan | (mV) | | (mm/y) | (mV) | |
| Ti1 | −298.2 | 0.934 | 3.43 | 369.6 | 2.27 | Ti2 | −69 | 1.6 | 5.88 | 338 | 1.8 | Ti64 | −220 | 0.708 | 2.65 | 427.3 | 0.597 | TiOs | −193.3 | 0.222 | 0.64 | 322.1 | 0.00531 | Ti15Mo | −139.9 | 4.68 | 15.67 | 133.7 | 3.19 | TMZF | −256.7 | 1.26 | 4.19 | 225.9 | 0.658 |
|
|