Research Article
Synthesis and Study of Electrical Properties of SbTeI
Table 1
SEM morphologies of compounds prepared under different conditions.
| Sample | SbTeI Growth conditions | SEM images of SbTeI Crystals | Crystal details |
| SbTeI-1 | Thermal treatment at 400°C for 480 hrs | | Size 2–8 m. Smooth rods stacked in random fashion. Enlarged micrograph shows hollow rods |
| SbTeI-2 | Thermal treatment at 600°C for 4 hrs | | Size 5–20 m. Mixture of rods, rectangular plates and, big plates |
|
|