Research Article
Effect on Mechanical and Thermal Properties of Random Copolymer Polypropylene/Microcrystalline Cellulose Composites Using T-ZnOw as an Additive
Table 4
Ea parameters of rPP and rPP based composites.
| (%) | Ea (kJ·mol−1) | rPP | MCC/rPP | MCC/PP-g-MA/rPP | T-ZnOw/MCC/PP-g-MA/rPP |
| 5 | 113.6 | 165.1 | 194.0 | 181.0 | 10 | 123.3 | 182.0 | 195.2 | 187.6 | 20 | 136.3 | 191.6 | 198.3 | 193.2 | 30 | 149.6 | 191.4 | 200.0 | 193.3 | 40 | 161.1 | 189.9 | 197.3 | 196.2 | 50 | 168.6 | 267.2 | 268.6 | 195.6 | 60 | 174.9 | 211.8 | 245.5 | 146.2 | 70 | 181.9 | 241.9 | 249.4 | 183.8 | 80 | 189.2 | 248.4 | 264.6 | 219.3 | 90 | 200.5 | 253.6 | 290.4 | - |
|
|