Review Article

Research Progress on Interlaminar Failure Behavior of Fiber Metal Laminates

Figure 18

X-ray images of the damage zone in samples with 1/8 in. Notch diameter of (a) type I hybrid FMLs and (b) type II hybrid FMLs [123].
(a)
(b)