Research Article

Numerical Simulation during Short-Shot Water-Assisted Injection Molding Based on the Overflow Cavity for Short-Glass Fiber-Reinforced Polypropylene

Table 2

The process parameters.

Melt short shot size (%)Water injection delay time(s)Melt temperature (°C)Water injection pressure(MPa)

7002104
7512306
8032508
85527010

Note: The numerical bolding in the table is the basic parameter to investigate the melt short shot size, water injection delay time, melt temperature, and water injection pressure.