Research Article

Effect of Oxidized Wood Pulp Fibers on the Performance of the Thermoplastic Corn Starch Composites

Table 1

The aldehyde contents of OWPF prepared at the different ratios of m(NaIO4)/m(WPF).

Sample no.Hydrolysis temperature (°C)Reaction temperature (°C)Reaction pHm(NaIO4)/m(WPF)CHO (%)

145504.00.1251.624
245504.00.2502.387
345504.00.3754.640
445504.00.5005.510