Research Article
Effect of Nanoclay Filler on Fatigue Life of Natural Rubber/Styrene-Butadiene Blend
Table 6
Storage modulus of samples.
| Temperature (°C) | Storage modulus (MPa) | | | S50N50 | S50N50C5 | S40N60 | S40N60C3 | S40N60C5 | S40N60C7 |
| -70 | 1313.15 | 934.78 | 633.95 | 276.55 | 175.15 | 230.37 | -50 | 30.68 | 12.65 | 45.37 | 28.38 | 12.93 | 10.75 | -30 | 7.39 | 10.02 | 8.09 | 8.21 | 10.38 | 8. 62 | -10 | 5.76 | 8.27 | 6.75 | 7.42 | 9.35 | 7.48 | 10 | 5.39 | 7.80 | 6.43 | 6.72 | 9.13 | 6.93 | 30 | 5.21 | 7.56 | 6.04 | 6.58 | 9.02 | 6.73 | 50 | 5.13 | 7.47 | 5.37 | 6.44 | 8.67 | 6.57 |
|
|