Research Article

Development of New PM Iron-Based Materials for Self-Lubricating Bearings

Figure 18

SEM micrographs of the marginal zone of the materials sintered at 900°C for 50 minutes: (a) 1% Sn; (b) 1.5% Sn; (c) 2.5% Sn.
248037.fig.0018