MaterialsSubstrateCrystal size (nm)Reference

Mn-doped CeO2CeCl3·H2O7.9–16.64[49]
CeO2@CCe(NO3)3·6H2O11.14–12.12[50]
CeO2, Ce1-xAgxO2Ce(NO3)3·6H2O18.8–140.9[51]
CeO2Ce(NO3)320–26.2[52]
CeO2Ce(NO3)3·6H2O10[53]
CeO2Ce(NO3)330–45[54]
CeO2CeCl3·7H2O12.53–16.07[47]
CeO2CeCl3·7H2O8.8–11.4This study