Electrospun Polyhydroxybutyrate and Poly(L-lactide-co-ε-caprolactone) Composites as Nanofibrous Scaffolds
Figure 5
Changes in the distribution of diameter of the fibre (μm) for electrospun scaffolds of (a) PHB; (b) PHB/PLCL at 75 : 25 (%, w/w); (c) PHB/PLCL at 50 : 50 (%, w/w); (d) PHB/PLCL at 25 : 75 (%, w/w); and (e) PLCL.