Synthesis and Characterization of Poly(lactic-co-glycolic) Acid Nanoparticles-Loaded Chitosan/Bioactive Glass Scaffolds as a Localized Delivery System in the Bone Defects
Figure 2
(a), (b), and (c) show higher magnification SEM micrographs of the S3 surface, respectively, after soaking in SBF solution for 7 days showing the apatite forming ability of the scaffolds.