Research Article
Long-Term In Vitro Degradation of a High-Strength Brushite Cement in Water, PBS, and Serum Solution
Figure 9
Representative histograms showing pore size distribution in cements degraded in H2O ((a) and (b)), in PBS ((c) and (d)), and in serum solution ((e) and (f)). The black lines show a fit to a lognormal distribution. The largest pores had a diameter of about 800 μm and typically 99.8% of the total number of pores had a diameter smaller than 100 μm.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |