Research Article

PMMA Third-Body Wear after Unicondylar Knee Arthroplasty Decuples the UHMWPE Wear Particle Generation In Vitro

Table 1

Size and shape of third-body particulate debris.

ParameterPorcine bone particlesPMMA particles

Mean diameter (µm)671.6 ± 186.4644.2 ± 262.6
ECD (µm)519.0 ± 142.9548.4 ± 237.3
FF0.41 ± 0.120.57 ± 0.12
AR1.74 ± 0.621.74 ± 0.70
Roundness0.50 ± 0.140.42 ± 0.14