Network parameters for HA-DVS cross-linked hydrogels and degradation level after 24 h of incubation with HAase.

[HA]HA/DVSDegradation level
%w.rPa(g/mol)(nm)%

52.5 : 1304.30971042642
5 : 156.022081073469
8 : 125.022382923877

62.5 : 1468.43612132435
5 : 1165.851104573168
8 : 142.452039583872

Value of the elastic modulus at 0.1 Hz.