Research Article

Fabrication of Poly(-caprolactone) Scaffolds Reinforced with Cellulose Nanofibers, with and without the Addition of Hydroxyapatite Nanoparticles

Table 2

Thermal properties of the produced scaffolds.

PCLPCL/CNFPCL/CNF/HANPp

(°C)<0.001
(°C)0.158
(j/g)0.019
0.107
(°C)0.038
Mass loss (%)<0.001

Significant difference from PCL; significant difference from PCL/CNF.