Research Article

Long-Term Fracture Resistance of Simulated Immature Teeth Filled with Various Calcium Silicate-Based Materials

Table 2

Mean fracture strengths (MPa) of teeth treated with BA, MTA-A, MTA-P, and ERRM at 24-month period and intergroup comparison of difference in fracture strength.

GroupsFracture strength
Mean ± SDMedian

1BA20.46 ± 2.5321.04 (15.78–23.31)0.005
2MTA-P18.88 ± 5.1317.45 (11.25–25.37)
3MTA-A14.12 ± 1.9913.61 (11.71–18.02)
4ERRM17.65 ± 4.2816.66 (12.57–26.37)

1-2 0.739
1-3 0.001
1-4 0.063
2-3 0.029
2-4 0.579
3-4 0.035

Kruskal-Wallis test; Mann-Whitney test; ; .