Research Article
Mechanical Properties and Biological Behavior of 3D Matrices Produced by Electrospinning from Protein-Enriched Polyurethane
Table 1
Electrospinning conditions for producing matrices from Tec-80A-GL blends.
| Blend composition | Electrospinning parameters | Voltage, kV | Solution supply rate, ml/h | Distance between spinneret and collector, cm |
| 3% Tec-80A + 5% GL | 19.0 | 1.3 | 20 | 3% Tec-80A + 10% GL | 18.5 | 1.3 | 20 | 3% Tec-80A + 15% GL | 18.5 | 1.2 | 19.5 | 3% Tec-80A + 20% GL | 20.0 | 1.2 | 19.5 | 5% Tec-80A + 5% GL | 19.5 | 1.3 | 20 | 5% Tec-80A + 10% GL | 22.5 | 1.4 | 20 | 5% Tec-80A + 15% GL | 21.0 | 1.4 | 18.5 | 5% Tec-80A + 20% GL | 20.0 | 1.3 | 18.5 | 7% Tec-80A + 5% GL | 21.0 | 1.5 | 20 | 7% Tec-80A + 10% GL | 22.1 | 1.3 | 20 | 7% Tec-80A + 15% GL | 24.0 | 1.2 | 19 | 7% Tec-80A + 20% GL | 24.0 | 1.0 | 19 |
|
|