Research Article

Properties Investigation of GO/HA/Pt Composite Thin Film

Figure 13

SEM micrographs of HA/GO/Pt coatings before and after corrosion tests (a, b) annealed at 200°C and (c, d) annealed at 600°C.

(a)
(b)
(c)
(d)