Antireflective Nanocomposite Based Coating on Crystalline Silicon Solar Cells for Building-Integrated Photovoltaic Systems
Table 2
Simulated solar cell’s parameters after curve fitting with experimental reflectance curve, refractive index, and thickness of ARNAB coating.
| Sample | ARC thickness (nm) | ARC r.i* | Broad band reflectance (%) | Isc (A) | Voc (V) | η (%) |
| #120001B (without ARC) | — | — | — | 2.53 | 0.64 | 13.5 | #121006 fed blue | 125 | 1.85 | 7 | 3.10 | 0.66 | 17.02 | #121008A yellow | 175 | 1.85 | 1 | 2.99 | 0.65 | 16.03 | #121010 magenta | 205 | 1.83 | 2 | 2.92 | 0.65 | 16.09 | #120703B blue | 94 | 1.85 | 5 | 3.40 | 0.65 | 18.82 | #121006B green blue | 250 | 1.85 | 1.5 | 3.00 | 0.65 | 16.51 | #120706B dark blue | 100 | 1.85 | 1.2 | 3.49 | 0.65 | 19.35 |
|
|
ARC: antireflective coating;
*r.i: refractive index; η: efficiency.
|