Summary of experimental materials and conditions used.

SolventDeionised water0.1 M acetic acid0.01 M HCl, 0.003 M HNO30.1 M HCl, 0.03 M HNO3
Sample ID70°C, 1 bar batch100°C, 200bar batch200°C, 250 bar flow-through70°C, 1 bar batch150°C, 200 bar batch250 °C, 250 bar flow-through100°C, 200 bar batch100°C, 200 bar batch200 °C, 200 bar batch

HTLMix
HTL315
HTL319
HTL321
HTL322
HTL324