Research Article
Performance Evaluation of STARPAM Polymer and Application in High Temperature and Salinity Reservoir
Table 8
Resistance coefficient and residual resistance coefficient of three polymers.
| Sample | Core parameters | | | C / mg/L | Number | L / cm | R / cm | V / cm3 | ϕ / % | K / 10−3μm2 | μ / mPa·s |
| STARPAM | S-1 | 5.92 | 2.50 | 8.25 | 28.39 | 1476 | 18.6 | 22.35 | 2.36 | 800 | STARPAM | S-2 | 5.99 | 2.51 | 8.33 | 28.16 | 1506 | 22.6 | 29.36 | 3.28 | 1000 | STARPAM | S-3 | 5.92 | 2.50 | 8.19 | 27.89 | 1466 | 45.2 | 38.56 | 4.67 | 1500 | MO-4000 | S-1 | 5.92 | 2.50 | 8.25 | 28.39 | 1476 | 9.6 | 12.32 | 1.45 | 800 | MO-4000 | S-2 | 5.99 | 2.51 | 8.33 | 28.16 | 1506 | 10.3 | 16.23 | 2.23 | 1000 | MO-4000 | S-3 | 5.92 | 2.50 | 8.19 | 27.89 | 1466 | 14.8 | 25.60 | 3.60 | 1500 | HAMP | S-1 | 5.92 | 2.50 | 8.25 | 28.39 | 1476 | 8.2 | 5.66 | 0.89 | 800 | HAMP | S-2 | 5.99 | 2.51 | 8.33 | 28.16 | 1506 | 9.6 | 12.32 | 1.22 | 1000 | HAMP | S-3 | 5.92 | 2.50 | 8.19 | 27.89 | 1466 | 12.6 | 20.13 | 2.63 | 1500 |
|
|
Remarks: L: length, R: diameter, V: pore volume, ϕ: porosity, K: permeability, μ: viscosity, : resistance coefficient, : residual resistance coefficient, and C: concentration. |