The used 3D-printing and curing parameters.
| Parameter | |
| Material feed pressure | 16.9 Psi | Printing spacing | 125 microns | Printing angle | 0° | Inner diameter of tip | 125 microns | Number of printed layers | 1 | Curing | 60°C, 30 minutes |
|
|