FTIR peak positions of various functional groups before and after composite formation.

Functional groupsIR peak positions (cm-1)
CSCSPHAp particlesHAp/CSP

1092, 1030, 6041079, 1025, 602
P–OH1088, 1047, 991, 4931070, disappeared, 984, disappeared
O–H bending632, 3571625, 3563
O–H stretching3430342734223402
N–H3467, 1622, 15443465, 1620, 15443462, 1620, 1543