XRR curves of the samples oxidized by (a) anodic oxidation at 20 V with and without heat treatment; (b) anodic oxidation at 40 V with and without heat treatment; (c) thermal oxidation in air at 500°C and 600°C.
(a) |
(b) |
(c) |