The comparison between the mean of phase transformation (m-phase fraction) Vol% values and their respective standard deviation of all the three groups, that is, Upcera, Ziecon, and Cercon, within each subgroup.

Upcera Ziecon Cercon value (significance < 0.05)

Comparison in between subgroups without artificial aging
Mean (%) ± SD6.08 ± 1.166.49 ± 0.7712.6 ± 1.150.00

Comparison in between subgroups with artificial aging
Mean (%) ± SD11.4 ± 1.911.0 ± 0.1814.3 ± 0.700.04