Research Article

Modulus of Elasticity of Two Ceramic Materials and Stress-Inducing Mechanical Deformation following Fabrication Techniques and Adhesive Cementation Procedures of a Dental Ceramic

Figure 1

The graph shows the mean of maximum mechanical deflection of the two dental ceramics (IPS e.max® Press glass-ceramic and Vitadur Alpha) characterized by profilometric measurements after polishing (A Pol), after stress relief (A Sr), after alumina air-particle abrasion (A aPb), and after resin cement coating at 0 hr, 24 hrs, 48 hrs, and 168 hrs (A C 0 hr, A 24 hrs, A 48 hrs, and A 168 hrs, respectively). (data from [16]).