Research Article

Breakdown and Evolution of the Protective Oxide Scales of AISI 304 and AISI 316 Stainless Steels under High-Temperature Oxidation

Figure 9

The SEM micrograph of the cross-section of AISI 316 corroded at °C in synthetic air at different magnifications: (a) 500x and (b) 2000x.
824676.fig.009