Research Article

Six-Year Evaluation of Thermal-Sprayed Coating of Zn/Al in Tropical Marine Environments

Figure 7

Thermal-sprayed coating of Zn/Al, sealed with wash primer 1 (345 μm). (a) 12 months of exposure. (b) 24 months of exposure. (c) 36 months of exposure. (d) 41 months of exposure. (e) 71 months of exposure.
318279.fig.007a
(a)
318279.fig.007b
(b)
318279.fig.007c
(c)
318279.fig.007d
(d)
318279.fig.007e
(e)