Research Article

Environmental and Material Influences on the Stress-Corrosion Cracking of Steel in H2O–CO–CO2 Solutions

Figure 10

Reduction in area as a function of the applied electrochemical potential at 800 kPa and 45°C with a gas mixture of 25% CO and 75% CO.
414156.fig.0010