Environmental and Material Influences on the Stress-Corrosion Cracking of Steel in H2O–CO–CO2 Solutions

Figure 7

Elongation and reduction in area as a function of temperature for specimens machined transverse to the rolling direction, at 800 kPa with a gas mixture of 50% CO and 50% CO2.