Research Article

Determination of Susceptibility to Intergranular Corrosion of UNS 31803 Type Duplex Stainless Steel by Electrochemical Reactivation Method

Figure 7

DLEPR curves plotted for DSS after solution and sensitization heat treatments at 725°C between 100 and 31622 min (scan rate: 15 V/hr).
651829.fig.007a
(a)
651829.fig.007b
(b)