Research Article

Deposition of Cerium-Based Conversion Coatings on Aluminum Alloy 380

Figure 7

Surface morphology of coatings deposited on panels rinsed at 100°C after immersion in the coating solution for (a) 2 min, (b) 5 min, (c) 8 min.
760284.fig.007a
(a)
760284.fig.007b
(b)
760284.fig.007c
(c)