Research Article

Deposition of Cerium-Based Conversion Coatings on Aluminum Alloy 380

Figure 9

Optical images of coatings deposited on substrates rinsed at 100°C (a) as deposited, and after salt spray testing for (b) 24 hours, (c) 96 hours, and (d) 192 hours.
760284.fig.009a
(a)
760284.fig.009b
(b)
760284.fig.009c
(c)
760284.fig.009d
(d)