Research Article
Corrosion Behaviour of Heat-Treated Aluminum-Magnesium Alloy in Chloride and EXCO Environments
Table 11
Electrochemical corrosion rate for the 1.23% Mg specimen.
| (sec) | NaCl solution | FeCl3 | EXCO solution | As-cast | RRA | As-cast | RRA | As-cast | RRA |
| 0 | 0 | 0 | 0 | 0 | 0 | 0 | 1200 | 0.0115 | 0.0057 | 0.0298 | 0.0234 | 0.0234 | 0.0119 | 2400 | 0.021 | 0.0105 | 0.0565 | 0.0435 | 0.0435 | 0.0222 | 3600 | 0.0302 | 0.0148 | 0.0816 | 0.0628 | 0.0616 | 0.0308 | 4800 | 0.0386 | 0.0185 | 0.1068 | 0.0805 | 0.0805 | 0.0394 | 6000 | 0.0750 | 0.0216 | 0.1283 | 0.0985 | 0.0965 | 0.0482 | 7200 | 0.0530 | 0.0401 | 0.1509 | 0.1158 | 0.1133 | 0.0554 |
|
|