Research Article

Anodic Dissolution of Spheroidal Graphite Cast Iron with Different Pearlite Areas in Sulfuric Acid Solutions

Table 3

Kinetic parameters of typical mechanisms for iron dissolution reaction.

Pieces of literature

Heusler et al. [18ā€“20] 2
Bockris et al. [15] 1
Abdul Azim and Sanad [37] 1

Note: is the anodic Tafel slope, and is the reaction order with respect to the hydroxyl ion activity.