Research Article

Effect of High Temperature Sodium Hydroxide Immersion on Fusion Bond Epoxy Coating

Figure 3

EDAX (Na element mapping) analysis of Fusion bond Epoxy coating exposed to 5% NaOH solution for 30 days at 93°C/200°F.