Research Article
Hot Corrosion of SrTiO3 Perovskite in Na2SO4 + 50 wt.% V2O5 and Na2SO4 + 10 wt.% NaCl Environments at 900°C
Figure 1
XRD patterns of the SrTiO3, (A) before exposure to hot corrosion and after exposure to hot corrosion at 900°C in (B) Na2SO4 + 50 wt.% V2O5 environment and (C) Na2SO4 + 10 wt.% NaCl environment.