Research Article
Study of the Corrosion Process of AZ91D Magnesium Alloy during the First Hours of Immersion in 3.5 wt.% NaCl Solution
Figure 8
Transverse profiles obtained from the CLSM micrographs of the AZ91D alloy: (a) the as-received condition; (b) after immersion for 15 h in 3.5 wt.% NaCl solution at room temperature.
(a) |
(b) |