Research Article
Prevention of Reinforcement Corrosion in Concrete by Sodium Lauryl Sulphate: Electrochemical and Gravimetric Investigations
Figure 3
Nyquist plots and Bode plots of steel reinforcement in concrete (a) in the absence and (b) presence of SLS for 160, 320, and 480 days.
(a) |
(b) |