Investigation of Mild Steel Corrosion in the Cement Production Associated with the Usage of Secondary Fuels
Figure 14
DSC tracks for goethite with decomposition to hematite, which was confirmed by the Raman spectroscopy. In case of lepidocrocite as starting product, maghemite (γ-Fe2O3) was primarily formed.