Research Article

Investigation of Mild Steel Corrosion in the Cement Production Associated with the Usage of Secondary Fuels

Figure 8

SEM images and corresponding EDX spectra; (a–c) referring to the outer surface of the upper, loose CP layer of sample M6/2 (spectrum of EDX1 not shown), (d–f) referring to the lower, adherent CP layer of sample M6/2, and (g–h) referring to the integral layer of M18/1. Spectra regions beyond 10 keV (right edge of the diagram) were free of any signals and, hence, cut off.
(a)
(b)
(c)
(d)
(e)
(f)
(g)
(h)