Research Article
Kinetics of Thermal Degradation of Recycled Polyvinyl Chloride Resin
Table 3
ln(
) (g/min°K) of recycled PVC resin at different times (min) and at different temperatures (100–140°C).
| (°K) | ln() (g/min°K) At different curing time (min) | Time = 10 min | Time = 20 min | Time = 30 min | Time = 40 min | Time = 50 min |
| 0.00268 | −9.94825 | −9.46949 | −9.6638 | −9.51551 | −9.38219 | 0.00261 | −9.62852 | −9.17355 | −9.48085 | −9.48285 | −9.36512 | 0.002544 | −8.89706 | −9.09667 | −9.30756 | −9.41183 | −9.3087 | 0.00248 | −8.78497 | −9.00963 | −9.26774 | −9.3072 | −9.23095 | 0.00242 | −8.54597 | −9.0009 | −9.24037 | −9.23906 | −9.15079 |
|
|