The amount of carbon elemental compositions (wt.%) on external surface supports and catalysts after reaction obtained from EDX (the spent catalyst used in the reaction condition at T = 200–400°C for 8.5 hr).

SampleTiO2-SGTiO2-SVWO3/TiO2-SGWO3/TiO2-SV

C (%)1.01.21.84.5